Production of Injection Outsole is simple and less-consuming process, which yields various advantages that Outsole can replace rubber Outsole. As being reached Rubber Outsole Grade thru high Injection & Material technology, Injection Outsole has both strong points from Injection (Light-Weight) & Rubber (Grip/Abrasion). Hereby, physical grade of Injection Outsole is approaching the main production stage and is expected to fulfill other industry requirements sooner or later.
PROPERTY |
UNIT |
OS-500 |
Hardness |
C Type |
68 ~ 73 |
Specific Gravity |
g/cm 3 |
Max 0.43 |
Elasticity |
% |
Min 43 |
Compression Set |
% |
Max 40 |
Shrinkage |
% |
Max 1.2 |
Tear Strength |
Kg/cm |
Min 22 |
Split Tear |
Kg/cm |
Min 3.5 |
Tensile Strength |
Kg/cm 2 |
Min 50 |
Elongation |
% |
Min 400 |
Abrasion (DIN) |
mm 3 |
Max 100 |
Abrasion (Akron) |
cc loss |
Max 0.15 |
Remark |
|
|
|
|
|
|
|
| |
|
|
|